Specifications: 

Crystal Structure: Cubic

Growth Method: Vernuil Method

Lattice Parameter: a=3.905Å

Nd Doping Concentrations: 0.05%

Melting Point: 2080C

Density: 5.122 g/ccm

Hardness: 6-6.5 Mohs

Thermal expansion: 9.4 x 10^-6/K

Dielectric Loss: ~5×10^-4 (300k), ~3×10^-4 (77k)

Sizes Available: 10×3m, 10×5m, 10×10mm, 15×15mm, 20×15mm, other sizes are available upon request

Orientations: <100>, <110>, <111>  

Miscut: 0.5 degree

Polish: single or double sided

Packing: Packing in class 1000 clean room with class 100 grade plastic bag 