MSE PRO™ Bare nickel cobalt manganese oxide lithium NCM622 polycrystalline (uncoated)
Product Details:
Lithium-ion cathode electrode material, which is uncoated NCM622 polycrystalline lithium nickel cobalt manganese oxide, is difficult to process and requires strict control of moisture content
Specifications
| Test item | Unit | Specifications | Actual measurement results | Testing methods or instruments |
| Li | wt% | 7.2±2.0 | 7.49 | |
| Ni+Co+Mn | wt% | 60.0±2.0 | 60.18 | |
| Ca | wt% | ≤0.01 | 0.0028 | ICP |
| Cu | wt% | ≤0.0001 | 0.0001 | ICP |
| Fe | wt% | ≤1.5 | 0.003 | ICP |
| Mg | wt% | ≤0.005 | 0.0033 | ICP |
| Na | wt% | ≤0.001 | 0.0105 | ICP |
| Zn | wt% | / | 0 | ICP |
| Free lithium | wt% | ≤0.5 | 0.0454 | Acid burette |
| D10 | µm | ≥6.0 | 7.25 | Laser particle size analyzer |
| D50 | µm | 9.0~12.0 | 11.26 | Laser particle size analyzer |
| D90 | µm | ≤20.0 | 17.64 | Laser particle size analyzer |
| BET | m2/g | ≥0.1 | 0.196 | Fully automatic surface area and porosity analyzer |
| TD | g/cm3 | ≤2.5 | 2.23 | Vibrating density measuring instrument |
| pH | / | ≤12.0 | 11.75 | pH value |
| Moisture | ppm | ≤150.0 | 86.8 | Moisture meter |
-
Packaging requirements:
Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags
Storage requirements: Sealed, stored in a cool and dry place. The material needs to be vacuum sealed for storage. The electrolyte used during testing is NCM electrolyte (KLD-1230C)
Baking conditions for electrode: Bake at 85 ℃ for 4 hours