MSE PRO Bare nickel cobalt manganese oxide lithium NCM523 polycrystalline (uncoated)
Couldn't load pickup availability
Consumables Product
This consumable product is not available for refund or return
Still have questions? Ask our experts!
MSE PRO™ Bare nickel cobalt manganese oxide lithium NCM523 polycrystalline (uncoated)
Specifications
| Test item | Unit | Test result | Test Method |
| Appearance | Black powder | ||
| D50 | (μm) | 11.5 | ICP |
| Specific surface area | (m²/g) | 0.28 |
BET; Specific surface area meter |
| Tap Density | (g/cm³) | 2.35 | Vibrating density meter |
| First reversible capacity | (mAh/g) | 160.1 | 0.1/0.1C (4.3-2.8V) |
| First effect | (%) | 84.8 | |
| Moisture | ppm | N/A | Karl Fischer Kulenfa |
| PH | N/A | 11.47 | PH value |
-
Packaging requirements:
Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags
Storage requirements: Sealed, stored in a cool and dry place. The material needs to be vacuum sealed for storage. The electrolyte used during testing is NCM electrolyte (KLD-1230C)
Baking conditions for electrode: Bake at 85 ℃ for 4 hours