LSAT Crystal Substrates, (La,Sr)(Al,Ta)O3 Crystal,  MSE Supplies

LSAT Crystal Substrates, (La,Sr)(Al,Ta)O3 Crystal

To better serve you, we would like to discuss your specific requirement, Please Contact Us for a quote.

Specifications:  

Growth method: Czochralski method

Crystal structure: Cubic

Lattice parameter: a = 3.868 A

Melt point (℃): 1840

Density: 6.74(g/cm3)

Hardness: 6.5(mohs)

Dielectric constants: 22

Thermal expansion: 10 x 10-6 /K

Available Size: 10x3,10x5,10x10,15x15,20x15,20x20,Ф15,  Ф20,Ф1″ (1 inch),Ф2″ (2 inch), Ф2.6″ (2.6 inch). Special sizes and orientations are available upon request.

Thickness: 0.5mm, 1.0mm

Polishing: Single or double

Crystal Orientation: <100>, <110>, <111> ±0.5º

Miscut: ±0.5°

Ra: ≤5Å (5µm × 5µm area)

Packaging: Packing in class 1000 clean room with class 100 grade plastic bag