{"product_id":"boron-doped-diamond-on-silicon-substrate-15mm-x-15mm-x-0-5mm","title":"Boron-Doped Diamond on Silicon Substrate-15mm x 15mm x 0.5mm-1 pc","description":"\u003ch2\u003eBoron-Doped Diamond on Silicon Substrate-15mm x 15mm x 0.5mm-1 pc\u003c\/h2\u003e\n\u003ch3\u003e\u003cstrong\u003e\u003cspan lang=\"EN-US\" style=\"font-size: 11.0pt; line-height: 107%; font-family: 'Calibri',sans-serif; mso-ascii-theme-font: minor-latin; mso-fareast-font-family: Calibri; mso-fareast-theme-font: minor-latin; mso-hansi-theme-font: minor-latin; mso-bidi-font-family: 'Times New Roman'; mso-bidi-theme-font: minor-bidi; color: red; mso-ansi-language: EN-US; mso-fareast-language: EN-US; mso-bidi-language: AR-SA;\"\u003eBuy Redox.me products from MSE Supplies at the best value.\u003c\/span\u003e\u003c\/strong\u003e\u003c\/h3\u003e\n\u003ch3\u003e\u003cspan\u003eDescription\u003c\/span\u003e\u003c\/h3\u003e\n\u003cp\u003e\u003cspan\u003eA Boron-Doped Diamond (BDD) on Silicon Substrate (Si) is a high-performance material that combines the excellent properties of diamond with the versatility of silicon. The substrate consists of a conductive silicon wafer that is coated with a thin layer of boron-doped diamond. Boron doping introduces p-type conductivity to the diamond layer, enhancing its electrical properties and making it suitable for use in electrochemical applications.\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003eOnly the front surface and the sides of the wafer are coated with BDD. \u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003eThis material offers a unique combination of attributes, including the high thermal conductivity, electrical conductivity, and hardness of diamond, along with the well-established compatibility and cost-effectiveness of silicon. Therefore, this product is a more affordable alternative to \u003c\/span\u003e\u003ca href=\"https:\/\/redox.me\/products\/boron-doped-diamond-plate-bdd-plate?_pos=1\u0026amp;_sid=c90d6f5c3\u0026amp;_ss=r\" title=\"Boron-doped diamond plate for electrochemistry\" rel=\"noopener\" target=\"_blank\"\u003epolycrystalline Boron-Doped Diamond Plate\u003c\/a\u003e\u003cspan\u003e. The boron doping further improves the substrate's ability to support electrochemical reactions, offering efficient charge transport and heat dissipation.\u003c\/span\u003e\u003c\/p\u003e\n\u003ch3\u003eApplication Notes\u003c\/h3\u003e\n\u003cp\u003e\u003cspan\u003eProperties of BDD are particularly important in electroanalysis for the development of sensors and biosensors. BDD electrodes allow to detect many electroactive molecules in aqueous media that would otherwise be masked by water decomposition reactions at higher potentials. The surface of BDD electrode can be further (photo)functionalized or decorated. In order to enhance the electrochemical response in a presence of organic molecules, the surface of BDD can be also modified with metal nanoparticles (e.g. Au). BDD is also a broadly used electrode material for electrochemical energy storage, electrocatalysis or electrosynthesis.\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003ePlease note that this product differs slightly in electrochemical properties from the polycrystalline Boron-Doped Diamond Plate. However, in most applications, using this product as a more affordable alternative is fully justified.\u003c\/span\u003e\u003c\/p\u003e\n\u003ch3\u003eSpecifications\u003c\/h3\u003e\n\u003ctable\u003e\n\u003cthead\u003e\n\u003ctr\u003e\n\u003cth\u003e\u003cstrong\u003eParameter\u003c\/strong\u003e\u003c\/th\u003e\n\u003cth\u003e\u003cstrong\u003eSpecification\u003c\/strong\u003e\u003c\/th\u003e\n\u003c\/tr\u003e\n\u003c\/thead\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003ctd\u003eThickness tolerance\u003c\/td\u003e\n\u003ctd\u003e\u0026lt; 10%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eOxygen evolution potential (0.5 M H₂SO₄)\u003c\/td\u003e\n\u003ctd\u003e2.3 V\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eHydrogen evolution potential (0.5 M H₂SO₄)\u003c\/td\u003e\n\u003ctd\u003e−0.8 V\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eBackground current\u003c\/td\u003e\n\u003ctd\u003e12 µA\/cm²\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eBoron doping concentration\u003c\/td\u003e\n\u003ctd\u003e1–5 × 10²⁰ cm⁻³\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eResistivity\u003c\/td\u003e\n\u003ctd\u003e37 Ω·cm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eBDD layer thickness\u003c\/td\u003e\n\u003ctd\u003e8 µm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eGrain size\u003c\/td\u003e\n\u003ctd\u003e7 µm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eRecommended long-term current density\u003c\/td\u003e\n\u003ctd\u003e\u0026lt; 80 mA\/cm²\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eElectrochemically active surface area\u003c\/td\u003e\n\u003ctd\u003e1.8 cm²\/cm²\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eOperational pH range\u003c\/td\u003e\n\u003ctd\u003e1–13\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003cp\u003e\u003cspan\u003e\u003cstrong\u003eMSE offers a range of electrodes. Please \u003ca href=\"https:\/\/support.msesupplies.com\/hc\/en-us\/\"\u003econtact us\u003c\/a\u003e for more information.\u003c\/strong\u003e\u003c\/span\u003e\u003c\/p\u003e","brand":"Redox.me","offers":[{"title":"Default Title","offer_id":41365438070842,"sku":"E-BDD(1)\/Si-15x15x0.5","price":980.95,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0722\/7785\/files\/BDD_1_Si_93bbeebb-0eef-481b-8e5b-f4290238fb2f.png?v=1777069383","url":"https:\/\/www.msesupplies.com\/en-gb\/products\/boron-doped-diamond-on-silicon-substrate-15mm-x-15mm-x-0-5mm","provider":"MSE Supplies","version":"1.0","type":"link"}